Package size per unit product 32.50cm * 32.50cm * 36.00cm Gross weight per unit product 21.000kg About Water Based Ink W
SHARE

Description

Basic Info
Model NO. FKD-2007
Performance Viscosity
Component Varnish, Color Paste, Asistant Liquid
Basic Color Red, Yellow, Blue, Black
Application PP Woven Cement Bag
pH Value 8.5-9.5
Waterproof 0 Grade
Wear Reisistance 0 Grade
Viscosity 20-25 Seconds Zahn Cup 3#
Deliver Time Within One Week
Custom Color Available
Stock Available
Features Good Adhesion, Scratch Resistance
Drying Type Quick Drying
MOQ 10kgs
Odor B Grade
Shelf Time 2 Years
Custom Sample Acceptable
Transport Package Barrel, Pallet
Specification 10kg/barrel, 20kg/barrel, 200kg/barrel
Trademark Oriental Colors
Origin China
HS Code 32159090
Production Capacity 700000 Kg/Month
Packaging & Delivery
Package size per unit product 32.50cm * 32.50cm * 36.00cm Gross weight per unit product 21.000kg
Product Description
About Water Based Ink
Water based ink is Made of water-soluble resin, organic pigment, solvent and related auxiliaries by grinding and stirring. The solid content is 40~50% (pigmeng+resin). Suitable for the printing of food paper packaging, plastic shopping bag, thermal paper label,corrugated paper carton, non woven fabric bag, woven bag (heavy industrial bag), plastic film,PLA film, FFS film, medical paper packaging.Environmentally friendly( no pollution), health(no harm to human), safe(non flamable), economy(savenatural resource).

PP Woven Bag High Gloss Water Based Printing Ink

PP Woven Bag High Gloss Water Based Printing Ink

Application fieldSquare bottom valve pocket, paper plastic bag, feed bag, cement bag, fertilizer bag
Machine TypeSuitable for CI flexo press, inline flexo press printing and high speed printing.
Product Parameter
Viscosity 3# zahn cuppH ValueFineness(μm)Wear ResistanceHeat Resistance(ºC)
14-208-9<550 times/4 pounds<230
Printing Parameter
Lines Per Inch(LPI)printing speed(MM)Doting Print 3# zahn cupsolid print 3# zahn cupviscosity can be adjusted accord to actual use
200-50050-24010-1313-16
Packaging10kg/bucket, 20kg/bucket,1000kg/bucket
Using instructionPlease stir evenly before using,keep the product ingredient consistent, test and adjust product pH value and viscosity, check color, keep the water based ink moving during using to prevent the ink from drying or plate blurring
Storage condition10-35ºC storaged in cool ventilated place, sealed, avoid fire, avoid rain
Shelf timesealed, one year

PP Woven Bag High Gloss Water Based Printing Ink

PP Woven Bag High Gloss Water Based Printing Ink

PP Woven Bag High Gloss Water Based Printing Ink


FAQ

Q1:How to avoid color difference?
A: Use new ink each time. Avoiding water adding, if it is needful, try to add little each time and mix evenly. Use the same substrate each time(the base color of the substrate will cause color difference. Maintain the printing press, anilox roller, andscraper in time; clean the ink box in time.Q2: Why there is odor from the ink?
A: Tap water will shorten the ink shelf time. It will deteriorate easier if too much tap water added. Stock the ink in sealed condition and in ventilated place.
Q3: How to solve the edge fluffing problem?
A: In low printing speed, restart the press or tune the press until the scraping plate appears. In normal high speed printing, add slowing dry agent or stabilizer to solve the fluffing problem.Q4: What are the reasons for the printed words are too slim and not clear?
A: The printing is too slow but drying is fast, poor converting. Printing pressure is too big and the ink loading is too much.Q5: The printing drying condition is not good, what are the reasons?
A: The ambient temperature is too low; the humidity is too high;the power of the drying tunnel or infrared lamp is low. Substrate surface is too smooth, and the ink absorption deviate.Q6: The ink become thick after long storage, how can I reuse it?
A: Generally speaking, if stored in our suggested way, the ink will keep in good condition. It become thick because it is stored unsealed and the water volatilized. you can add some stabilizer and water, stir evenly and filter. Then you can use again.